Atomic layer deposition (ALD)
Films grown one atomic layer at a time, coating deep features evenly.
- Position
- Winning
- Checked on
- 25 Nov 2026
Chip insulators and linersRoutine, growing
Each new transistor generation adds layers.
Theses that rest on this
What it is
Two gases take turns. The first sticks to the surface until every spot is covered, then stops; the excess is pumped away. The second reacts with that layer. Each cycle adds a fixed sliver, about 0.11 nm for aluminium oxide (Wikipedia). Because each step stops by itself, the film is the same thickness at the bottom of a deep trench as at the top.
The number: 100 to 300 nm an hour for aluminium oxide, the price of that control (Wikipedia).
The read
Fair potential, high readiness: slow, but the only way to coat the tiny, deep structures of new transistors and memory, so its share grows with each generation. The tool market is led by one firm.
The catchThroughput. Thick films by ALD cost far more tool time than by other methods.
How it scores
Potential48
Impact 2
If it works fully, who would notice?
Without it, chips would fall a generation behind on their specification sheets.
Intel used ALD for its gate insulators from 45 nm in 2007, and DRAM makers need it below 100 nm (Wikipedia). Buyers would see slower, leakier chips.
Judgement
Novelty 4
Would a buyer switch for it, all else equal?
Coats deep, narrow features evenly where other methods leave thin spots.
For DRAM below 100 nm it is described as the only usable method (Wikipedia). Other methods still make the job's thicker films, at far higher rates. Close to 3.
Judgement
Readiness75
Viability 5
Does it do the job it is sold for?
Routine in every leading chip fab, from several tool makers.
Logic and DRAM makers have used it in volume for nearly two decades (Wikipedia). ASM, Beneq and Picosun sell the tools (Wikipedia).
Independent
Drivers 3
Who is pulling, and how hard?
Repeat orders at the going price.
Gate-all-around transistors need more ALD layers with each generation; ASM expects its ALD and epitaxy markets to grow 9% to 13% a year to 2030 (Quartr, Dec 2025). Buyers do not commit ahead.
Maker's claim
Ease of adoption 4
Given that it works, how much must the adopter change?
Fabs already run it; each new film needs qualifying.
A new ALD layer fits existing tools and lines; the wait is testing the recipe.
Judgement
Supply 4
Could a buyer get it if one country or one firm said no?
Four or more tool makers in volume.
ASM holds more than 55% of the market (Quartr); the other large tool makers sell the rest. Close to 3.
Judgement
The brakeCostSlow growth makes thick films dear.
What changed
- 1974 Tuomo Suntola devises the method in Finland Where it began Context Wikipedia
- 2007 Intel reports ALD gate insulators in 45 nm chips A layer only ALD could make forced fabs to adopt it Viability up to 5 Wikipedia
- 19 Feb 2025 Lam launches a molybdenum ALD tool for volume production Metal wiring moves to ALD; Lam claims up to 50% lower resistance than tungsten Drivers holds at 3 Silicon Semiconductor
- 15 Dec 2025 ASM says its ALD share passed 55% in 2024 One leader, several rivals Supply holds at 4 Quartr
Who captures the value
The tool makers, ASM above all, and the chemical firms that make the precursor gases. Chipmakers buy the tools as part of each new line. ASM's market for single-wafer ALD is forecast at $5.1 to $6.1 billion by 2030 (Quartr).
What would change this
- 2027Second-generation gate-all-around chips in volume. More ALD layers would test drivers at 4.
- Any dateALD that grows only where wanted, cutting a lithography step. Would move novelty.
Prediction65%
ASM still holds more than half the ALD tool market in its 2027 annual report.
Against the alternatives
The alternatives table is on the deposition page.
Who is involved
- Choices a buyer has
- At least three tool makers (Wikipedia).
- Funded challengers
- None counted.
| Name (country, listing) | Role | Money | Stage |
|---|---|---|---|
| ASM International (Netherlands, Euronext) | makes tools | part of ASM | Over 55% share |
| Applied Materials (US, Nasdaq) | makes tools | part of Applied | In volume |
| Lam Research (US, Nasdaq) | makes tools | part of Lam | Molybdenum ALD in volume |
| Tokyo Electron (Japan, Tokyo) | makes tools | part of TEL | In volume unverified |
| Micron (US, Nasdaq) | buys | part of Micron | Early user of molybdenum ALD |
| Intel (US, Nasdaq) | buys | part of Intel | ALD gate insulators since 2007 |