# Atomic layer deposition (ALD)

Source: https://stateofthefuture.io/manufacturing/chipmaking-equipment/ald-atomic-layer-deposition/
Checked: 25 Nov 2026

Films grown one atomic layer at a time, coating deep features evenly.

Potential 48. Readiness 75. Position: Winning.

## What it is

Two gases take turns. The first sticks to the surface until every spot is covered, then stops; the excess is pumped away. The second reacts with that layer. Each cycle adds a fixed sliver, about 0.11 nm for aluminium oxide ([Wikipedia](https://en.wikipedia.org/wiki/Atomic_layer_deposition)). Because each step stops by itself, the film is the same thickness at the bottom of a deep trench as at the top.

The number: 100 to 300 nm an hour for aluminium oxide, the price of that control ([Wikipedia](https://en.wikipedia.org/wiki/Atomic_layer_deposition)).

Cost: Research tools cost about $200,000 to $800,000 ([Wikipedia](https://en.wikipedia.org/wiki/Atomic_layer_deposition)); production tool prices are not public.

What counts: every form of ALD on wafers, including plasma and spatial ALD. Crystal growth is on [epitaxy](https://stateofthefuture.io/manufacturing/chipmaking-equipment/epitaxy/).

## The read

Fair potential, high readiness: slow, but the only way to coat the tiny, deep structures of new transistors and memory, so its share grows with each generation. The tool market is led by one firm.

The catch: Throughput. Thick films by ALD cost far more tool time than by other methods.

## How it scores

- **Impact 2/5.** Without it, chips would fall a generation behind on their specification sheets.. Intel used ALD for its gate insulators from 45 nm in 2007, and DRAM makers need it below 100 nm ([Wikipedia](https://en.wikipedia.org/wiki/Atomic_layer_deposition)). Buyers would see slower, leakier chips. Judgement
- **Novelty 4/5.** Coats deep, narrow features evenly where other methods leave thin spots.. For DRAM below 100 nm it is described as the only usable method ([Wikipedia](https://en.wikipedia.org/wiki/Atomic_layer_deposition)). Other methods still make the job's thicker films, at far higher rates. Close to 3. Judgement
- **Viability 5/5.** Routine in every leading chip fab, from several tool makers.. Logic and DRAM makers have used it in volume for nearly two decades ([Wikipedia](https://en.wikipedia.org/wiki/Atomic_layer_deposition)). ASM, Beneq and Picosun sell the tools ([Wikipedia](https://en.wikipedia.org/wiki/Atomic_layer_deposition)). Independent
- **Drivers 3/5.** Repeat orders at the going price.. Gate-all-around transistors need more ALD layers with each generation; ASM expects its ALD and epitaxy markets to grow 9% to 13% a year to 2030 ([Quartr, Dec 2025](https://quartr.com/events/asm-international-nv-asm-investor-day-2025_oj7A3gqv)). Buyers do not commit ahead. Maker's claim
- **Ease of adoption 4/5.** Fabs already run it; each new film needs qualifying.. A new ALD layer fits existing tools and lines; the wait is testing the recipe. Judgement
- **Supply 4/5.** Four or more tool makers in volume.. ASM holds more than 55% of the market ([Quartr](https://quartr.com/events/asm-international-nv-asm-investor-day-2025_oj7A3gqv)); the other large tool makers sell the rest. Close to 3. Judgement

The brake: Cost. Slow growth makes thick films dear.

## What changed

- 1974: Tuomo Suntola devises the method in Finland. Where it began [Wikipedia](https://en.wikipedia.org/wiki/Atomic_layer_deposition)
- 2007: Intel reports ALD gate insulators in 45 nm chips. A layer only ALD could make forced fabs to adopt it [Wikipedia](https://en.wikipedia.org/wiki/Atomic_layer_deposition)
- 19 Feb 2025: Lam launches a molybdenum ALD tool for volume production. Metal wiring moves to ALD; Lam claims up to 50% lower resistance than tungsten [Silicon Semiconductor](https://siliconsemiconductor.net/article/121172/Lam_Research_ushers_in_new_era_of_semiconductor_metallisation_)
- 15 Dec 2025: ASM says its ALD share passed 55% in 2024. One leader, several rivals [Quartr](https://quartr.com/events/asm-international-nv-asm-investor-day-2025_oj7A3gqv)

## Who captures the value

The tool makers, ASM above all, and the chemical firms that make the precursor gases. Chipmakers buy the tools as part of each new line. ASM's market for single-wafer ALD is forecast at $5.1 to $6.1 billion by 2030 ([Quartr](https://quartr.com/events/asm-international-nv-asm-investor-day-2025_oj7A3gqv)).

## What would change this

- 2027: Second-generation gate-all-around chips in volume. More ALD layers would test drivers at 4.
- Any date: ALD that grows only where wanted, cutting a lithography step. Would move novelty.

Prediction: ASM still holds more than half the ALD tool market in its 2027 annual report. Probability 65%.

## Against the alternatives

The alternatives table is on [the deposition page](https://stateofthefuture.io/manufacturing/chipmaking-equipment/deposition/).

## Who is involved

| Name (country, listing) | Role | Money | Stage |
| --- | --- | --- | --- |
| ASM International (Netherlands, Euronext) | makes tools | part of ASM | Over 55% share |
| Applied Materials (US, Nasdaq) | makes tools | part of Applied | In volume |
| Lam Research (US, Nasdaq) | makes tools | part of Lam | Molybdenum ALD in volume |
| Tokyo Electron (Japan, Tokyo) | makes tools | part of TEL | In volume [unverified] |
| Micron (US, Nasdaq) | buys | part of Micron | Early user of molybdenum ALD |
| Intel (US, Nasdaq) | buys | part of Intel | ALD gate insulators since 2007 |


Author: Lawrence Lundy-Bryan, State of the Future (https://stateofthefuture.io/)